  【塑料球】塑料空心球,塑胶球价格,塑料小球生产厂家POM塑料球(POM塑胶球)PA塑料球(尼龙塑料球)PP塑料球(塑料PP球)PMMA塑料球(PMMA塑胶球)PC塑料球(PC塑胶球)PVC塑料球(PVC塑胶球)PPA塑料球(PPA塑胶球)PSU塑料球(PSU塑胶球)玩具塑料球(儿童玩具球)饰品塑料球(饰品塑胶球)塑料空心球(空心塑胶球)生物降解塑料球(PLA塑料球)软胶塑料球(软胶塑胶球)PEEK塑料球(PEEK塑胶球)PTFE塑料球(特氟龙塑料球)TPX塑料球(TPX塑胶球)Pepper ball0.68 Pepperball塑料焊接技术解决方案塑料热板焊接技术塑料超声波焊接技术塑料激光焊接技术塑料摩擦焊接技术实心塑料球(实心塑胶球)POM实心塑料球(POM塑料球)PA实心塑料球(PA塑料球)实心PP塑料球(塑料PP球)PMMA实心塑料球(PMMA塑料球)PVC实心塑料球(PVC塑料球)PTFE实心塑料球(特氟龙塑料球)塑料小球,塑料小球厂家精密塑料球焊接技术解决方案塑料激光焊接实用技术塑料热板焊接实用技术塑料超声焊接实用技术塑料球行业新闻,塑胶球新闻塑料空心球(空心塑料球)PTFE空心塑料球(PTFE空心球)PC空心塑料球(PC空心球)POM空心塑料球(POM塑料球)TPX空心塑料球(TPX空心球)PP空心塑料球(塑料空心PP球)PA空心塑料球(PA空心球)塑料浮球(塑胶浮球)PE空心球塑料球规格,塑胶球规格游戏塑料球,游戏塑胶球塑料空心球规格,空心塑胶球规格塑胶球标准,塑料球标准塑料空心球标准,空心塑胶球标准塑料球规格尺寸,塑胶规格尺寸塑料球硬度测试方法,塑胶球测试空心塑料球密度测试方法塑胶球规格,塑料球规格橡胶球,硅胶球,橡胶球价格,硅胶球厂家橡胶球-硅胶球厂家硅胶球,食品级硅胶球硅胶洗衣球-硅胶球厂家橡胶洗衣球-硅胶球厂家空心硅胶球,空心橡胶球橡胶弹力球橡胶球规格,硅胶球规格橡胶密封圈塑料球阀电动塑料球阀(电动塑胶球阀)塑料浮球阀(塑胶浮球阀)塑料法兰球阀(塑胶法兰球阀)氟塑料球阀(氟塑胶球阀)塑料三通球阀(塑胶三通球阀)胡椒球,胡椒弹0.43英寸塑料彩弹0.68英寸塑料彩弹0.68英寸胡椒球Pepper ball0.68 pepper ball0.50 pepper ball taiwan0.43 peper ball japanBB弹
产品简介 首页 > 产品简介 >  
 
 
0.68car Factors affecting the density of solid plastic pepperball
 
 
 
详情
 

The density of solid plastic pepper balls can't be exactly the same due to the differences in materials and injection molding technology. For customers with low requirements, the existence of such differences doesn't have much impact, but some customers with high requirements require that the density of solid plastic pepper balls should be consistent, so we should find out the reasons for the difference.

In the process of injection molding, the solid plastic pepper ball is easy to make gas remain in the plastic pepper ball and form bubbles, which are the main reasons that affect the density of the plastic hollow pepper ball. The main reasons for the bubbles in the middle of the plastic solid pepper ball are the material, the mold and the parameter setting of the injection molding machine.

The main reason for the material is that the material is not fully dried, which causes the gas in the material to enter the mold cavity with the rubber compound and form bubbles. The improvement method is to fully dry the material, which will completely solve the bubbles in the plastic pepper ball caused by the moisture in the material.

In the original drawing of the mold, because the gas in the runner of the plastic pepper ball mold did not leave the mold in time, this part of the gas was trapped inside the plastic pepper ball and formed bubbles. The solution is to exhaust the mold accordingly, and the gas in the mold will be exhausted outside the mold, so that bubbles will not be formed.

In the process of injection molding of injection molding machine, the shooting speed of the machine is too fast, so that the gas in the mold can not be discharged from the mold in time, resulting in trapped gas and bubbles. The solution is to slow down the shooting speed of the injection molding machine, which can significantly solve the problem of bubbles in plastic pepper balls.



 